Skip to content

FGF Printer

These are the FAST group's own lab signs. They are written for one lab, its equipment, its layout and its local procedures, and are published so others can see and adapt them. They are not general safety guidance and they are not a substitute for training.

If you work somewhere else, follow your own workplace procedures and the requirements of your institution and jurisdiction.

reviewawaiting PI, post-doc, equipment owner or subject-matter reviewv0.1 · review owner: PI / post-doc · updated 2026-11-14
  • This is a GreenBoy3D pellet extruder on a converted Prusa MK3S in TEB7. It takes granulate feedstock instead of filament and is a specialty machine, not a shared printer.
  • STOP. Do not use this printer without express permission and training from the PI or a post-doc.
  • Training covers the extruder, the feedstock rules, purging, and the waste route. Being trained on the FFF printers does not carry over.
  • NEVER flash stock Prusa firmware onto this printer. It runs a fork with changed probe offsets, E-steps, thermistor table and travel limits. Stock firmware drives the head into the bed and misreads temperature.
Feedstock Use Notes
Virgin pellets, PLA or PETG Yes Confirm the material is dry.
FAST recycled shred, PLA or PETG, known history Yes, within the reprocessing limit Check the container label. See below.
Any polymer other than PLA or PETG NEVER This printer is set up for PLA and PETG only. Ask first.
Unknown polymer, mixed polymer, or unlabelled container NEVER Unknown melt behaviour and unknown fumes. Ask.
Anything with metal, grit, labels, adhesive, or dirt in it NEVER Wrecks the auger and barrel. Re-sort or discard it.
Anything outside 0.3 to 5 mm NEVER Oversize bridges and jams the auger. In-house shred is sieved to 3 mm.
  • Keep feedstock containers closed and labelled with polymer and cycle count.
  • Wet feedstock prints badly and can spit. Dry it if it has been open to room air.
  • General practice: PLA at 45 °C for 4 to 6 hours, PETG at 60 °C for 6 hours. Do not dry PLA hotter. It softens near 60 °C and loose shred will fuse into a solid lump.

Every melt degrades the polymer, so recycled stock is not indefinitely reusable. A cycle is one trip through a melt. Virgin pellets printed once are cycle 1; shred from those prints, printed again, is cycle 2.

  • The container label is the log. Write the polymer and the cycle number on every feedstock container, and increment it when a batch is shredded and refilled.
  • Single-source PLA or PETG: up to 3 cycles.
  • Mixed-source shred: up to 2 cycles.
  • Past that, or if the label is missing or the count unknown, treat the batch as non-structural only, or ask before using it at all.
  • Wear eye protection when loading or unloading the machine, and any time the enclosure doors are open.
  • Check the hopper is clear and holds the feedstock you expect. Do not mix polymers in a hopper.
  • Confirm the previous user purged the barrel, or purge it yourself before starting.
  • Check the nozzle, barrel, and heater wiring look undamaged.
  • Have a metal tray or container ready for purge material.
  • Check the bulk hopper has enough feedstock for the print, and that its feed tube is clear.
  • Check the enclosure door closes and the HEPA fan runs.
  • The barrel runs hotter and holds far more heat than an FFF hotend. Treat every metal part of the extruder as hot.
  • NEVER put fingers or tools into the hopper or feed throat while the printer is powered. Clear blockages only when the machine is off and you have been trained to do it.
  • Purge material comes out hot and in quantity. NEVER let it land on your hand or the floor. Aim it into a tray; the bed works but makes more cleanup.
  • NEVER leave a print running unattended, and no overnight runs. If you have to leave, stop the print.
  • Stop the print if the extruder grinds, stalls, runs empty, smokes, or smells wrong.
  • Do not restart the same failing job without finding the cause. A repeated jam damages the auger and barrel.
  • Pellets and shred on the floor are a slip hazard. Sweep up spills immediately.
  • Keep feedstock off the floor and off walkways.
  • Do not return floor-swept material to a feedstock container. It is contaminated.
  • This machine extrudes far more plastic per hour than a filament printer, and shred emits more ultrafine particles than virgin pellets.
  • Run with the enclosure door closed and the HEPA filter fan on.
  • Purge, failed prints, and clean single-polymer offcuts go back to FAST polymer recycling if the polymer is known. See the Waste Disposal sign.
  • Contaminated, mixed, or unknown material does not go into polymer recycling.
  • Leave the printer, hopper area, and bench clean and clear for the next user.
  • Report printer problems rather than leaving them for the next user.

Source: lab-signs/printers-fgf.md · equipment record · all signs and records